02/02/2026
Cold Weather Concrete placement has a process that must be followed to have success. We pre-heated the ground the day before our pour to be sure it was over 35 degrees at the time of pouring. Went with 4,000psi + Calcium for a quicker set of the concrete. Once set up we cut expansion joints and covered the slab in concrete freeze blankets.
We will allow the blankets to stay in place for minimum 7 days to ensure proper curing of the concrete. Reach out with any questions or help with your next project!